Waterborne high build alkyd finish
Edit:Chenyang Group Created:2009-10-15 17:31:37

Characteristics:
a. Good mechanical strength;
b. Excellent anticorrosive resistance, thick-painted performance, one spraying can up to 60 µm or more;
c. Good adhesion.
Introduction:
Waterborne high build alkyd finish is recognized by the U.S. ASTM Standards, and accord with the waterborne coating standard promulgated by .the Ministry of Railways. Refined by modified water-based resin, pigments and fillers, driers, special additives and water.
Application:
Used in light industry, wood, vehicles, ships, bridges, construction and other industries.
Technical parameters:
Item | Index | |
Color & Appearance | Fit the standard sample plateand its color shading extent, level and smooth | |
VOC content (ASTM Standard) | ≤160 | |
Sagging resistance | 250 μm wet film thickness is no sagging | |
Viscosity (3# , 6 r/min) PaS | 2.5-8.0 | |
Solid content % | ≥55 | |
Fineness μm | ≤45 | |
Bending property mm | ≤4 | |
Grid test grade | ≤1 | |
Drying time | Surface drying (h) | ≤3.0 (25℃) |
Hard drying (h) | ≤24 (25℃) | |
Cupping test (mm) | ≥4.0 | |
Freeze-thaw stability (cycle) | 5 | |
Water resistance (48h) | No blistering, no rusting, lightly gloss is allowed | |
Coating method:
High pressure airless spraying or air spraying.
Direction for use:
- Stirred uniformly before use, in general case, do not need mix with other materials, if the viscosity is high and difficult to construct, added a small amount of water properly, stirred well before construct;
- The coating material should be degreasing, derusting, decontaminating and other treatments in accordance with national standards or industry standards before coating;
- Maintain pH 7.5-8.5;
- Do not construct when high humidity or rainy days.
Storage and transportation:
Storage time: 6 months. Store in a cool well-ventilated place, avoid sunlight, and 5℃-35℃; Avoid cold, sun exposure and rain when transporting.
Other products of waterborne antirust paint: